Search results
1651
[Page extract]
ASTM F1566-09
These test methods cover recognized methods for testing mattress innersprings, boxsprings, and finished mattresses or mattress sets, or both, to ensure uniformity of results.
1652
[Page extract]
ASTM D7617/D7617M-11
This test method specifies the test requirements for (FRP) composite smooth round rods and textured bars for determining the transverse shear strength via a double shear fixture.
1653
[Page extract]
IEC 61196-1-308
IEC 61196-1-308:2012(E) applies to coaxial communication cables. It specifies test methods for tensile strength and percentage elongation at fracture for annealed and hard-drawn solid copper clad metals to be used as inner conductor for coaxial cables.
1654
[Page extract]
ASTM D2261
This test method covers the measurement of the tearing strength of textile fabrics by the tongue (single rip) procedure using a recording constant-rate-of-extension-type (CRE) tensile testing machine.
1655
Case study
Prüfung des Verschlusses des hygienischen Abfallbehälters
Beispiel für kundenspezifisches Engineering Ein Hersteller von Hygienebehältern kam mit einer Windelentsorgungseinheit zu uns, die mit einem Drehansaugmechanismus ausgestattet war.
1656
[Page extract]
ASTM C158
These test methods cover the determination of the modulus of rupture in bending of glass and glass-ceramics. These test methods are applicable to annealed and prestressed glasses and glass-ceramics available in varied forms.
1657
[Page extract]
ISO 10123
Specifies a method for the determination of the shear strength of anaerobic-curing liquid adhesives used for retaining cylindrical assemblies, pin-and-collar type, or for locking and sealing threaded fasteners.
1658
[Page extract]
BS EN 12814-6
BS EN 12814-6 is a low temperature tensile test method for testing welded joints of thermoplastics semi-finished products.
1659
[Page extract]
ASTM D1321
This test method covers the empirical estimation of the consistency of waxes derived from petroleum by measurement of the extent of penetration of a standard needle.
1660
Page
Sie haben den Mecmesin-Newsletter abonniert
Danke
Wir wünschen Ihnen viel Spaß mit den regelmäßigen Updates zu unseren Entwicklungen bei Kraft-, Material- und Drehmomentprüfungen.
1662
Event
Wine & Spirits Capping: Cork Pull & Twist Caps
Wine packaging has a great influence on the quality of the product delivered to the customer.
1663
[Page extract]
BS EN 60352-2
Solderless connectors, Electric connectors, Crimped connectors, Electrical components, Electronic equipment and components, Electrical connections, Communication equipment, Crimping tools, Dimensions, Mechanical crimping, Dimensional measurement, Electr
1664
[Page extract]
ASTM D2105
ASTM D2105 determines the comparative longitudinal tensile properties of fiberglass pipe when tested under defined conditions of pretreatment, temperature, and testing machine speed.
1665
[Page extract]
ASTM E1820-18ae1
The ASTM E1820 test method covers procedures and guidelines for the determination of fracture toughness of metallic materials using the following parameters: K, J, and CTOD (δ). Toughness can be measured in the R-curve format or as a point value.
1666
[Page extract]
ASTM D2718
These test methods determine the shear properties of structural panels associated with shear distortion of the planes parallel to the edge planes of the panels. Both shear strength and modulus of rigidity may be determined.
1667
[Page extract]
BS EN ISO 23907
Test methods for various aspects of sharps bin safety requirements. Relevant to us are Penetration test and possibly Handle strength
1668
[Page extract]
ASTM D2370
This test method covers the determination of the elongation, tensile strength, and stiffness (modulus of elasticity) of organic coatings when tested as free films.
1669
[Page extract]
ASTM D5169-98
This test method measures the shear strength of hook and loop touch fasteners using a recording constant rate of extension (CRE) tensile testing machine.
1670
[Page extract]
ASTM D5170-98
This test method covers the measurement of the peel strength of hook and loop touch fasteners using a recording constant-rate-of-extension tensile testing machine (CRE).
1671
[Page extract]
BS 1726-1
Provides guidance on methods of specifying and tolerancing hot coiled compression springs, and cold coiled springs that fall outside the size range limits specified in BS EN 15800.
1672
[Page extract]
ISO 20795-1
ISO 20795-1:2013 classifies denture base polymers and copolymers and specifies their requirements. It also specifies the test methods to be used in determining compliance with these requirements.
1673
Case study
Kostengünstige Prüfung der Kabelstärke
Beispiel für kundenspezifisches Engineering Ein bedeutender Hersteller von Kabelbäumen und Steckverbindern wandte sich an uns, um eine kostengünstige Lösung für Zugkraftprüfkabel mit unterschiedlichen Durchmessern und direkt gebondeten Verbin
1674
[Page extract]
ISO 34-2
ISO 34-2 specifies a method for the determination of the tear strength of small test pieces (Delft test pieces) of vulcanized or thermoplastic rubber.
1675
[Page extract]
BS EN 3475-505