Search results
1251
[Page extract]
ASTM D1871
This test method is used to test the strength of adhesion of single-filament wire to vulcanized rubber compounds. It applies to wire made from brass, bronze or zinc coated steel wire.
1252
[Page extract]
ASTM D380
ASTM D380 is a set of test methods for determining testing and inspection procedures for rubber hoses e.g. hydraulic hoses and automotive hoses.
1253
[Page extract]
BS EN 1393
BS EN 1393 specifies a test method for testing the longitudinal tensile properties of glass-reinforced thermosetting plastics (GRP) pipes.
1254
[Page extract]
SAE J174
This test procedure is intended to provide a quality control method for checking torque-tension characteristics of non-prevailing torque type threaded steel fasteners 1/4 through 1 in nomial diameters.
1255
[Page extract]
ASTM D7137 / D7137M-17
ASTM D7137 is a test method that measures the compression residual strength properties of multidirectional polymer matrix composite laminated plates, which have been subjected to quasi-static indentation
1256
[Page extract]
ASTM D2659
ASTM D2659 determines the mechanical properties of blown thermoplastic containers under columnar crush conditions at a steady rate of compression. Any container, whether blown commercially or in the laboratory, may be used as the test specimen.
1257
[Page extract]
BS EN 1465
Specifies a method for determining the tensile lap-shear strength of bonded assemblies when tested on a standard specimen and under specified conditions of preparation and testing.
1258
[Page extract]
ISO 7810
Stipulates test method as per ISO/IEC 10373-1 for determining the Peel Strength of cards.
1259
[Page extract]
ASTM D3410 / D3410M
ASTM D3410 determines the compressive properties of polymer matrix composite materials reinforced by high-modulus fibers.
1260
[Page extract]
ISO 8510-1
Particularly suitable for use with less flexible adherends for which a 180 ° peel test is not suitable because the adherends crack, break or delaminate. A bonded assembly of two adherends is prepared using the adhesive under test.
1261
[Page extract]
BS EN ISO 8670-2
Two part test on filled bags:
1) 20 N tensile flange seal test, pulled in two directions in turn, at 180 degrees, in shear plane across flange, bag held by transparent custom plate
1262
[Page extract]
ISO 594-2
ISO 594 and EN 1707 contain 8 separate tests, some of which are only applicable to Luer lock fittings. Most of these tests require that the sample be assembled to a particular precision steel reference fitting.
1263
[Page extract]
PSTC 8
Unwind adhesion is a quantitative measure of the degree of ease or difficulty in unwinding a roll of tape.
The test specimen shall be any 10 m (10 yard) or more roll of pressure sensitive tape - preferably 24 mm (1”) wide.
1264
[Page extract]
ASTM C158
These test methods cover the determination of the modulus of rupture in bending of glass and glass-ceramics. These test methods are applicable to annealed and prestressed glasses and glass-ceramics available in varied forms.
1265
[Page extract]
ASTM F1566-09
These test methods cover recognized methods for testing mattress innersprings, boxsprings, and finished mattresses or mattress sets, or both, to ensure uniformity of results.
1266
[Page extract]
ASTM D7617/D7617M-11
This test method specifies the test requirements for (FRP) composite smooth round rods and textured bars for determining the transverse shear strength via a double shear fixture.
1267
[Page extract]
ASTM D1321
This test method covers the empirical estimation of the consistency of waxes derived from petroleum by measurement of the extent of penetration of a standard needle.
1268
[Page extract]
ASTM E8/E8M-13a
These test methods cover the tension testing of metallic materials in any form at room temperature, specifically, the methods of determination of yield strength, yield point elongation, tensile strength, elongation, and reduction of area.
1269
[Page extract]
ISO 1798
ISO 1798 specifies a method for determining the strength and deformation properties of flexible cellular materials when a test piece is extended at a constant rate until it breaks.
This test standard is equivalent to BS EN ISO 1798:2008
1270
[Page extract]
BS EN 520
Plasterboard, Gypsum plaster, Boards, Wall linings, Construction systems parts, Performance, Strength of materials, Fire resistance, Sound insulation, Water vapour, Permeability, Thermal resistance, Performance testing, Dimensional measurement, Physical
1271
[Page extract]
ISO 505
ISO 505 specifies a method of test for the measurement of the propagation resistance of an initial tear in textile conveyor belts, either in full thickness or of the carcass only.
1272
[Page extract]
ISO 813
ISO 813 specifies a method for the determination of the adhesive strength of a vulcanized or thermoplastic rubber bonded to a rigid substrate, using a test piece comprising a strip of rubber bonded to a single plate of rigid material.
1273
[Page extract]
ASTM D816-06
These test methods cover tests to measure the properties of adhesives, commonly called rubber cements, that may be applied in plastic or fluid form and that are manufactured from natural rubber, reclaimed rubber, synthetic elastomers, or combinations of
1274
[Page extract]
ASTM F1147-05
This test method covers tension testing of calcium phosphate and metallic porous coatings adhering to dense metal substrates at ambient temperatures.